MIL-S-851-D
ADMENDMENT 1
31 August 1990
MILITARY SPECIFICATION
STEEL GRIT, SHOT, AND CUT WIRE SHOT;
AND IRON GRIT AND SHOT BLAST
CLEANING AND PEENING
This specificication is approved for use within
the Department of the Air Force and is available
for use by all Departments and Agencies of the
Department of Defense
This admendment forms a part of MIL-S-851D, dated 21 April 1989, and is approved
for use by all Departments and Agencies of the Department of Defense.
PAGE 2
2.1.1: DELETE
QQ-W-423 Wire, Steel, Corrosion Resisting
2.2: ADD:
Society of Automotive Engineers, Inc.
SAE J441 Cut wire shot, recommended practice
(SAE standards may be purchased from the Society of Automotive Engineers, Inc.,
400 Commonwealth Drive, Warrendale, PA 15096)
AMSC N/A FSC 5350
DISTRIBUTION STATEMENT A: Approved for public release; distribution is unlimited.
1 OF 2
INCH-POUND
Downloaded from http://www.everyspec.com
资源描述:

当前文档最多预览五页,下载文档查看全文

此文档下载收益归作者所有

当前文档最多预览五页,下载文档查看全文
温馨提示:
1. 部分包含数学公式或PPT动画的文件,查看预览时可能会显示错乱或异常,文件下载后无此问题,请放心下载。
2. 本文档由用户上传,版权归属用户,天天文库负责整理代发布。如果您对本文档版权有争议请及时联系客服。
3. 下载前请仔细阅读文档内容,确认文档内容符合您的需求后进行下载,若出现内容与标题不符可向本站投诉处理。
4. 下载文档时可能由于网络波动等原因无法下载或下载错误,付费完成后未能成功下载的用户请联系客服处理。
关闭